Effect of high temperature corrosion on austenitic stainless steel grade 304 in CO2 gas at 700ºC
Austenitic stainless steels of grade 304 were exposed to dry (Ar-75%CO2) and wet (Ar-75%CO2-12%H2O) environments at 700oC. This experimental setup involved horizontal tube furnace connected to CO2 gas and water vapour facilities. X-ray diffraction (XRD) technique, variable pressure-scanning electron...
Main Authors: | , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
Universiti Kebangsaan Malaysia
2014
|
Online Access: | http://journalarticle.ukm.my/7263/ http://journalarticle.ukm.my/7263/ http://journalarticle.ukm.my/7263/1/14_Nurul_Atikah.pdf |