Injectable hydroxyapatite - b-tricalcium phosphate – calcium sulphate biocement
Injectable biocement as bone substitute material for filling in parts of defect bone and capable of setting itself in the body was produced based on a mixture of 40-50% hydroxyapatite, 10-20% b-tricalcium phosphate and 40-60% calcium sulphate dehydrate. Two different liquids were used for the prepa...
Main Authors: | Wan Khartini Wan Khodir, Roslinda Shamsudin, Abdul Razak Daud, Yusof Abdullah |
---|---|
Format: | Article |
Published: |
Universiti Kebangsaan Malaysia
2005
|
Online Access: | http://journalarticle.ukm.my/3954/ http://journalarticle.ukm.my/3954/ |
Similar Items
-
Effect of hydroxyapatite and tricalcium phosphate addition
on protein foaming-consolidation porous alumina
by: Sopyan, Iis, et al.
Published: (2011) -
Concentration effect of aqueous synthesis on biphasic hydroxyapatite - β-tricalcium phosphate composition
by: Alqap, Asep Sofwan F., et al.
Published: (2010) -
Effect of hydroxyapatite and tricalcium phosphate addition
on protein foaming-consolidation porous alumina
by: Iis, Sopyan, et al.
Published: (2012) -
Recent developments on injectable calcium phosphate bone cement
by: Hablee, Sufiamie, et al.
Published: (2016) -
The effects of calcium excess,water amount and mixing time on the injectability of calcium phosphate filling materials
by: Alqap, Asep Sofwan F., et al.
Published: (2012)