Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure
Objectives: To evaluate the effect of simulated pulpal pressure (PP) on initial bond strength of one-stsep self-etch adhesives with different smear layer preparation. Methods: Flat coronal dentin surfaces were obtained from extracted molar teeth .Smear layers were created by grinding with either #18...
Main Authors: | , , |
---|---|
Format: | Conference or Workshop Item |
Language: | English English |
Published: |
2012
|
Subjects: | |
Online Access: | http://irep.iium.edu.my/44213/ http://irep.iium.edu.my/44213/ http://irep.iium.edu.my/44213/6/aadr2012.pdf http://irep.iium.edu.my/44213/11/2012-aadrlist.pdf |
id |
iium-44213 |
---|---|
recordtype |
eprints |
spelling |
iium-442132015-11-30T07:14:50Z http://irep.iium.edu.my/44213/ Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure Mahdan, Mohd. Haidil Akmal Masatoshi, Nakajima Junji, Tagami RK Dentistry Objectives: To evaluate the effect of simulated pulpal pressure (PP) on initial bond strength of one-stsep self-etch adhesives with different smear layer preparation. Methods: Flat coronal dentin surfaces were obtained from extracted molar teeth .Smear layers were created by grinding with either #180 or #600 grit paper. A HEMA-free one-step self-etch adhesive, Xeno V (XV; Denstply,Germany) and a HEMA-containing adhesive, Tokuyama Bond Force (TBF;Tokuyama Corporation,Japan) were applied to the dentin surfaces according to the manufacturer's instructions under a hydrostatic pressure of 0 or 15 cmH2O. Specimens bonded under 0 cmH20 pressure was served as a control group. After coronal build up with composite resin (CLEARFIL AP-X), the specimens were stored in water at 370C for 24 hour. Bond strength to dentin were determined using microtensile bond (TBS) testing and all data were statistically analyzed using one-way ANOVA (materials and experimental conditions) and additional t-test. Results: The bond strength values (TBS) results table are as follows. Bond Strength of HEMA-free And HEMA-containing Adhesives Under Pulpal Pressure. Available from: http://www.researchgate.net/publication/266777476_Bond_Strength_of_HEMA-free_And_HEMA-containing_Adhesives_Under_Pulpal_Pressure [accessed Dec 1, 2015]. 2012 Conference or Workshop Item PeerReviewed application/pdf en http://irep.iium.edu.my/44213/6/aadr2012.pdf application/pdf en http://irep.iium.edu.my/44213/11/2012-aadrlist.pdf Mahdan, Mohd. Haidil Akmal and Masatoshi, Nakajima and Junji, Tagami (2012) Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure. In: American Asoociation of Dental Research 2012 (AADR Annual Meeting), 21-24 March 2012, Tampa,USA. (Unpublished) https://iadr.confex.com/iadr/2012tampa/webprogram/Paper156443.html |
repository_type |
Digital Repository |
institution_category |
Local University |
institution |
International Islamic University Malaysia |
building |
IIUM Repository |
collection |
Online Access |
language |
English English |
topic |
RK Dentistry |
spellingShingle |
RK Dentistry Mahdan, Mohd. Haidil Akmal Masatoshi, Nakajima Junji, Tagami Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure |
description |
Objectives: To evaluate the effect of simulated pulpal pressure (PP) on initial bond strength of one-stsep self-etch adhesives with different smear layer preparation. Methods: Flat coronal dentin surfaces were obtained from extracted molar teeth .Smear layers were created by grinding with either #180 or #600 grit paper. A HEMA-free one-step self-etch adhesive, Xeno V (XV; Denstply,Germany) and a HEMA-containing adhesive, Tokuyama Bond Force (TBF;Tokuyama Corporation,Japan) were applied to the dentin surfaces according to the manufacturer's instructions under a hydrostatic pressure of 0 or 15 cmH2O. Specimens bonded under 0 cmH20 pressure was served as a control group. After coronal build up with composite resin (CLEARFIL AP-X), the specimens were stored in water at 370C for 24 hour. Bond strength to dentin were determined using microtensile bond (TBS) testing and all data were statistically analyzed using one-way ANOVA (materials and experimental conditions) and additional t-test. Results: The bond strength values (TBS) results table are as follows.
Bond Strength of HEMA-free And HEMA-containing Adhesives Under Pulpal Pressure. Available from: http://www.researchgate.net/publication/266777476_Bond_Strength_of_HEMA-free_And_HEMA-containing_Adhesives_Under_Pulpal_Pressure [accessed Dec 1, 2015]. |
format |
Conference or Workshop Item |
author |
Mahdan, Mohd. Haidil Akmal Masatoshi, Nakajima Junji, Tagami |
author_facet |
Mahdan, Mohd. Haidil Akmal Masatoshi, Nakajima Junji, Tagami |
author_sort |
Mahdan, Mohd. Haidil Akmal |
title |
Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure
|
title_short |
Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure
|
title_full |
Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure
|
title_fullStr |
Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure
|
title_full_unstemmed |
Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure
|
title_sort |
bond strength of hema-free and hema-containing adhesives under pulpal pressure |
publishDate |
2012 |
url |
http://irep.iium.edu.my/44213/ http://irep.iium.edu.my/44213/ http://irep.iium.edu.my/44213/6/aadr2012.pdf http://irep.iium.edu.my/44213/11/2012-aadrlist.pdf |
first_indexed |
2023-09-18T21:02:53Z |
last_indexed |
2023-09-18T21:02:53Z |
_version_ |
1777410740864417792 |