Initial stage oxidation of cr in dry and wet environment at 1073 K and the significant differences of FT – IR spectra produced thereof
Little information has been known on the initial – stage oxidation if there is water vapor involved. Cr samples of 10 mm × 10 mm × 1 mm were isothermally oxidized in dry and wet environment respectively for 86.4 ks. Compact and even surface of Cr2O3 was formed on samples oxidized in dry environme...
Main Authors: | Kaderi, Akbar, Meskon, Shahrul Razi, Ani, Mohd Hanafi, Othman, Raihan |
---|---|
Format: | Article |
Language: | English |
Published: |
Trans Tech Publications, Switzerland
2012
|
Subjects: | |
Online Access: | http://irep.iium.edu.my/27471/ http://irep.iium.edu.my/27471/ http://irep.iium.edu.my/27471/1/Initial_stage_oxidation_of_cr_in_dry_and_wet_environment_at_1073_k_and_the_significant_differences_of_ftir_spectra_produced_thereof.pdf |
Similar Items
-
Observation on void formed in oxide scale of Fe-Cr-Ni alloy at 1073K in dry and humid environments
by: Kaderi, Akbar, et al.
Published: (2011) -
Studies on initial stage of high temperature oxidation of Fe - 9 to 12% Cr alloys in water vapour environment
by: Kaderi, Akbar, et al.
Published: (2012) -
Internal oxidation of Ni-Cr-Al alloys under various oxygen partial pressures at 1273 K
by: Ani, Mohd Hanafi, et al.
Published: (2012) -
The effects of water vapor on high temperature oxidation of Fe-Cr-Ni alloy at 1073k
by: Ani, Mohd Hanafi, et al.
Published: (2012) -
Formation of protective Cr2O3 scale at high temperature and the effect of mass transport in the presence of water vapor
by: Ani, Mohd Hanafi, et al.
Published: (2012)