Formation of protective Cr2O3 scale at high temperature and the effect of mass transport in the presence of water vapor
The formation of protective Cr2O3 scale at high temperature was evaluated using Wagner’s theory of binary alloy oxidation. The results show that at 1073 K, around 9.8 wt% of Cr is required to form external Cr2O3 scale, and 3.5wt% of Cr is needed to maintain the scale. Introduction of water vapor has...
Main Authors: | Ani, Mohd Hanafi, Othman, Raihan |
---|---|
Format: | Article |
Language: | English |
Published: |
Trans Tech Publications Ltd., Switzerland
2012
|
Subjects: | |
Online Access: | http://irep.iium.edu.my/16691/ http://irep.iium.edu.my/16691/ http://irep.iium.edu.my/16691/ http://irep.iium.edu.my/16691/1/Formation_of_protective_Cr2O3_scale_at_high_temperature.pdf |
Similar Items
-
Observation on void formed in oxide scale of Fe-Cr-Ni alloy at 1073K in dry and humid environments
by: Kaderi, Akbar, et al.
Published: (2011) -
Studies on initial stage of high temperature oxidation of Fe - 9 to 12% Cr alloys in water vapour environment
by: Kaderi, Akbar, et al.
Published: (2012) -
Microstructural evaluation and corrosion behaviour of Fe-Cr-Ni-Mn-Co AND AI0.5-Fe-Cr-Ni-Mn-Co highentropy alloys (HEA) with elemental additions / Siti Sarah Mohd Pauzi
by: Mohd Pauzi, Siti Sarah
Published: (2018) -
Effect of temperature on porosity of iron ore sinter with biochar derived from EFB
by: Purwanto, Hadi, et al.
Published: (2018) -
Internal oxidation of Ni-Cr-Al alloys under various oxygen partial pressures at 1273 K
by: Ani, Mohd Hanafi, et al.
Published: (2012)